Study on the Main Factors of Frequency Variation of LC Resonant Prestress Detection Method

Table 2

Ф9 mm experimental data of aluminum strands.

l/mf1 (kHz)f2 (kHz)f3 (kHz)f4 (kHz)SDRE (%)f (kHz)

6.0104.612104.625104.606104.6080.00860.0182104.613
6.5103.273103.277103.262103.2810.00820.0184103.273
7.0101.836101.847101.864101.8560.01220.0278101.851
7.5101.166101.179101.191101.1960.01340.0296101.183
8.0100.815100.784100.787100.7940.01400.0308100.795
10.098.42198.36398.46598.3970.04260.103098.411
10.597.62197.66697.64397.6330.01920.046497.641
11.097.00997.01497.01896.9940.01060.024797.009
11.596.35096.32696.33996.3650.01660.040596.345
12.095.70495.70795.71995.7050.00720.016495.709
12.594.96594.93894.93494.9510.01400.032694.947
14.094.18694.19994.17194.1840.01150.029794.185
14.593.54193.56693.54293.5470.01170.026793.549
15.093.21993.22893.21093.2220.00760.019793.220
15.592.67692.68092.66592.6760.00640.015892.674
16.092.48092.44892.49292.4650.01880.046992.471