Research Article

Research on Friction Stir Spot Welding Brazing Process and Properties of Dissimilar Metals DP590 and 6061

Table 2

Three factors and three levels selected in the orthogonal test.

LevelFactor
ABC
Rotating speed (r/min)Residence time (s)Pressing depth (mm)

11000600.1
21200900.2