Research Article

Performance Evaluation of Waste Crumb Rubber/Silica Fume Composite Modified Pervious Concrete in Seasonal Frozen Regions

Table 3

Compressive strength of RSFPC.

Mix IDCompressive strength (MPa)
123MeanSt. dev.

WCR4 + SF1223.922.824.423.70.67
WCR6 + SF1222.422.923.723.00.54
WCR8 + SF1220.520.119.119.90.59