Mechanical performance test of the polymer mortar.
| Strength under standard test conditions | Strength under weather test conditions | Curing age (d) | Flexural strength (MPa) | Compressive strength (MPa) | Folding ratio | Curing period | Flexural strength (MPa) | Compressive strength (MPa) | Folding ratio |
| 28 | 5.68 | 16.39 | 2.89 | — | — | — | — | 33 | 7.17 | 18.66 | 2.60 | 28d + 20H-R | 5.23 | 17.15 | 3.282 | 38 | 7.06 | 18.88 | 2.67 | 28d + 40H-R | 4.88 | 15.91 | 3.264 | 43 | 7.38 | 18.97 | 2.57 | 28d + 60H-R | 4.72 | 14.33 | 3.036 | 48 | 7.6 | 19.51 | 2.60 | 28d + 80H-R | 5.27 | 15.17 | 2.879 |
|
|