[Retracted] Optimization of Reinforced Aluminium Scraps from the Automobile Bumpers with Nickel and Magnesium Oxide in Stir Casting
Table 2
Results of the experiments.
| Experimental trail No. | Pressure (P) (MPa) | Time (t) (s) | Speed (N) (rpm) | Tensile strength (MPa) | Hardness (HRB) |
| ET 1 | 80 | 20 | 400 | 128.48 | 49.82 | ET 2 | 80 | 40 | 500 | 133.98 | 51.26 | ET 3 | 80 | 60 | 600 | 139.48 | 52.7 | ET 4 | 100 | 20 | 500 | 121.2 | 46.1 | ET 5 | 100 | 40 | 600 | 126.7 | 47.54 | ET 6 | 100 | 60 | 400 | 169.7 | 62.66 | ET 7 | 120 | 20 | 600 | 113.92 | 42.38 | ET 8 | 120 | 40 | 400 | 156.92 | 57.5 | ET 9 | 120 | 60 | 500 | 162.42 | 58.94 |
|
|