Experimental runs and responses.

A (rpm)B (mm)C (mm/min)D (l/min)Ra (microns)MRR (mm3/min)Pc (HP)

18500.2100064.2170.23610.207
18500.6200062.6501.29311.408
12000.4100064.7970.78260.751
25000.4200062.0700.74660.865
25000.4150042.7460.62490.635
12000.4200064.5500.86361.026
18500.4150063.4340.76460.808
18500.2150044.6460.19540.253
18500.4150063.4340.76460.808
18500.4150063.4340.76460.808
12000.2150065.3340.33510.425
25000.4150081.6420.78730.819
18500.2150083.5420.35780.437
25000.6150061.5341.19411.190
12000.4150084.1220.90430.981
18500.6100062.8971.21211.133
18500.4100044.1090.64290.578
18500.4200082.7580.88631.037
18500.4100083.0050.80530.762
12000.6150064.0141.31111.351
12000.4150045.2260.74190.796
25000.2150062.8540.21810.264
18500.6150082.2221.33381.363
18500.2200063.9700.31710.482
18500.4150063.4340.76460.808
18500.6150043.3261.17141.179
18500.4150063.4340.76460.808
18500.4200043.8620.72390.853
25000.4100062.3170.66560.590