Research Article

Experimental Study and Effect on Recycled Fibers Blended with Rotor/OE Yarns for the Production of Handloom Fabrics and Their Properties

Table 4

Pairwise comparison for unevenness (CVM %) values.

RawRaw materialsMean differenceStandard errorSignificanceLower boundUpper bound

100% VC25–75% VC–R−1.17830.6834330.785454−1.14701.6170
50–50% VC–R−1.77670.6834330.345023−0.74002.1167
75–25% VC–R1.86670.6834330.1610360.33973.3936
25–75% VC–R100% VC1.17830.6834330.785454−1.61701.4370
50–50% VC–R−0.59830.6834330.377549−0.83002.0267
75–25% VC–R−0.68830.6834330.1677680.24973.3036
50–50% VC–R100% VC1,77670.6834330.345023−2.11670.7400
25–75% VC–R0.59830.6834330.377549−2.02670.8300
75–25% VC–R−0.09000.6834330.233733−0.25002.2067
75–25% VC–R100% VC1.86670.6834330.161036−3.3936−0.3397
25–75% VC–R0.68830.6834330.167768−3.3036−0.2497
50–50% VC–R0.09000.6834330.233733−2.60670.2500