Microstructure and Performances for Wear-Resistant Steel through the WAAM Technology

Figure 13

Morphology of the sample at 500 (a, c, e, g, i) and 1000 (b, d, f, h, j) times magnifications subjected to wear tests at (a, b) 20 N, (c, d)25 N, (e, f) 30 N, (g, h) 35 N, and (i, j) 40 N loads.