Experiment on Size Effect and Fractal Characteristics of Waste Brick and Concrete Recycled Aggregate
Table 1
95% guarantee rate representative value of crushing strength of single particle.
| Aggregate type | Particle size (mm) | Maximum value (MPa) | Minimum value (MPa) | Average value (MPa) | Standard deviation (%) | Coefficient of variation (%) | 95% representative value of single-particle strength |
| Recycled brick | 9.5–16 | 3.93 | 1.81 | 2.916 | 86 | 29 | 1.49 | 16–19 | 2.6 | 1.61 | 2.168 | 39 | 18 | 1.51 | 19–26.5 | 2.48 | 1.62 | 1.772 | 37 | 21 | 1.15 | 26.5–31.5 | 2.21 | 0.88 | 1.371 | 54 | 40 | 0.46 |
| Recycled aggregate particles of concrete | 9.5–16 | 4.88 | 2.94 | 3.998 | 79 | 19 | 2.69 | 16–19 | 4.13 | 2.51 | 3.319 | 66 | 20 | 2.23 | 19–26.5 | 3.98 | 1.97 | 2.832 | 82 | 29 | 1.47 | 26.5–31.5 | 3.51 | 1.51 | 2.507 | 81 | 32 | 1.16 |
|
|