New Sodium Intercalation Cathode Prepared by Sodiation of Delithiated Host LiNi1/3Mn1/3Co1/3O2

Figure 2

(a) Initial charge curve (oxidation state) of LiNMC in half-cell Li | LiPF6 1M/EC-DMC (1 : 1) | LiNMC at C/25 rate. (b) First charge-discharge curve of NazNMC in half-cell Na | NaClO4/PC-FEC (98 : 2) | NazNMC.