Research Article
New Sodium Intercalation Cathode Prepared by Sodiation of Delithiated Host LiNi1/3Mn1/3Co1/3O2
Figure 3
Electrochemical behavior of the sodiated NazNMC in half-cell of Na || NaClO4/PC-FEC (98 : 2) || NazNMC. (a) CV curves at a scan rate of 0.1 mV s−1. (b) The galvanostatic charge–discharge profiles at the rate of C/25 and C/10. (c) The specific capacity and Coulombic efficiency versus cycles and (d) rate capability test.
| (a) |
| (b) |
| (c) |
| (d) |