Research Article

Multifeature Extraction of Three-Dimensional Topography of Carbon Steel Specimen during Fatigue Process

Table 3

Posterior probability values of test data.

Test data
Predicted loading cycles0 cycle2000 cycles4000 cycles6000 cycles8000 cyclesFacture

02.146 × 10−28.75 × 10−1612.624 × 10−7498.717 × 10−13959.498 × 10−4302≈0
20001.779 × 10−126.915 × 10−51.425 × 10−151.0 × 10−911.96 × 10−3919.313 × 10−1490
40002.06 × 10−3626.656 × 10−2124.947 × 10−34.33 × 10−4314.436 × 10−2808≈0
60002.13 × 10−7134.3 × 10−4559.0 × 10−1424.776 × 10−38.35 × 10−3084.799 × 10−1901
80003.9 × 10−7272.312 × 10−4001.558 × 10−1782.15 × 10−492.59 × 10−71.196 × 10−81
Fracture≈03.57 × 10−34591.19 × 10−32312.83 × 10−17432.877 × 10−6555.78 × 10−4