Research Article
Study on Synthesis and Service Properties of Anticoagulant Ice Microcapsule Coating Material
Table 4
Technical indices of emulsified asphalt.
| Test item | Test results | Technical standard | Experiment method |
| Particle charge | Cation | Anion | Cation | Anion | T0653 | Demulsification speed | Rapid rupture | Slow rupture | Rapid rupture | Slow rupture | T0658 | The remaining amount on the sieve (1.18 mm) (%) | 0.05 | 0.03 | ≤0.1 | ≤0.1 | T0652 | 5d storage stability (%) | 3.39 | 3.76 | ≤5 | ≤5 | T0655 | Standard viscosity of asphalt C25,3 (s) | 18 | 20 | 10–25 | 8–20 | T0621 | Evaporation residue content (%) | 58 | 59 | ≥50 | ≥50 | T0651 | Evaporation residue | Ductility (15°C) (cm) | 58.2 | 77.4 | 40 | 40 | T0605 | Penetration (25°C) (0.1 mm) | 71.6 | 76.2 | 50–200 | 50–300 | T0604 | Softening point (°C) | 50.7 | 50.4 | ≥50 | ≥50 | T0606 | Solubility (trichloroethylene) (%) | 98.6 | 59.2 | ≥97.5 | ≥97.5 | T0607 |
|
|