Study on Synthesis and Service Properties of Anticoagulant Ice Microcapsule Coating Material
Table 6
Bond strength results under different drawing rates.
| | Constant speed specimen | Bond strength (MPa) | | 20 mm/min | 15 mm/min | 10 mm/min | 5 mm/min |
| | Cationic emulsified asphalt test piece | 0.16 | 0.31 | 0.21 | 0.11 | | 1.27 | 0.88 | 0.66 | 0.12 | | Electrode difference | 1.11 | 0.57 | 0.45 | 0.01 | | Anionic emulsified asphalt test piece | 0.05 | 0.03 | 0.03 | 0.04 | | 0.66 | 0.25 | 0.14 | 0.06 | | Electrode difference | 0.61 | 0.22 | 0.11 | 0.02 |
|
|