Experimental summary of wear test.
| | Exp. runs | % of reinforcement | Applied load (N) | Disc speed (m/s) | Sliding distance (m) | Wear rate (mm3/m) |
| | 1 | 0 | 15 | 1.0 | 1000 | 0.572 | | 2 | 0 | 25 | 1.5 | 1200 | 0.379 | | 3 | 0 | 35 | 2.0 | 1400 | 0.792 | | 4 | 0 | 45 | 2.5 | 1600 | 0.823 | | 5 | 4 | 15 | 1.5 | 1400 | 0.548 | | 6 | 4 | 25 | 1.0 | 1600 | 0.697 | | 7 | 4 | 35 | 2.5 | 1000 | 0.418 | | 8 | 4 | 45 | 2.0 | 1200 | 0.815 | | 9 | 8 | 15 | 2.0 | 1600 | 0.734 | | 10 | 8 | 25 | 2.5 | 1400 | 0.483 | | 11 | 8 | 35 | 1.0 | 1200 | 0.392 | | 12 | 8 | 45 | 1.5 | 1000 | 0.582 | | 13 | 12 | 15 | 2.5 | 1200 | 0.676 | | 14 | 12 | 25 | 2.0 | 1000 | 0.228 | | 15 | 12 | 35 | 1.5 | 1600 | 0.346 | | 16 | 12 | 45 | 1.0 | 1400 | 0.286 |
|
|