Research Article

Fluxless Direct Soldering of Transparent Conductive Oxides (TCOs) to Copper

Figure 7

Fractography of an AZO/Cu joint with Sn8Zn3Bi1Mg active solder after shear tests at room temperature: (a) the Cu side; (b) the AZO side.
(a)
(b)