Research Article
Investigation on Microstructure and Tensile Properties of High-Strength AA2014 Aluminium Alloy Welds Joined by Pulsed CMT Welding Process
Table 4
Tensile test results of PCMT welded aluminium alloy joint.
| Joint No | Condition | Microhardness (HV) | 0.2% YS (MPa) | % elongation (50 mm gauge length) | UTS (MPa) | Efficiency (%) | WZ | HAZ |
| 1 | P-CMT welded joint | 88 | 75 | 258 | 6.3 | 303 | 67% | 2 | Base material | 155 | — | 431 | 9 | 455 | — |
|
|