Research Article

Effects of Process Parameters on Geometrical Characteristics and Microstructure of TiC Particle-Reinforced Co50 Alloy by Laser Cladding

Table 9

Preparation parameters and the corresponding sample numbers.

CoatingsComposition ratios, rm (Co50 : TiC)Laser power, P/kWScanning speed, (mm/min)Laser energy density, Pw/(kW.s/cm2)

A (A2)1 : 03.340012.57
B (B4)9 : 13.650010.97
C (C1)4 : 13.935016.98
D (D1)7 : 34.235018.29