Research Article
Fiber-Reinforced Magnesium Phosphate Cement-Based Nanocomposites in the Field of Bridge Structure Repair and Strengthening
Table 2
Summary of damaged beam bearing capacity.
| Beam number | Damage-cracking load | Cracking load of reinforcement layer | Ultimate load |
| AO-0 | 17.23 | ā | 35.69 | AO-1 | 16.12 | 28.65 | 62.15 | AO-2 | 15.23 | 24.65 | 45.36 |
|
|