Research Article
Fatigue Performance of Rubber Concrete in Hygrothermal Environment
Figure 13
Microstructures of the interfacial transition zone, subjected to (a) 0 wet-dry cycles, (b) 0 wet-dry cycles, (c) 14 wet-dry cycles at 20°C, (d) 14 wet-dry cycles at 60°C, (e) 21 wet-dry cycles at 20°C, (f) 21 wet-dry cycles at 60°C, (g) 28 wet-dry cycles at 20°C, and (h) 28 wet-dry cycles at 60°C.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |
(g) |
(h) |