Research Article
Fatigue Performance of Rubber Concrete in Hygrothermal Environment
Table 2
Technical indexes of rubber particle.
| Moisture content (%) | Ash content (%) | Acetone extract (%) | Metal content (%) | Fiber content (%) | Sieve residue content (%) | Tensile strength (MPa) | Elongation at break (%) |
| 0.62 | 8.75 | 5.12 | 0.02 | 0.00 | 0.014 | 16.8 | 564 |
|
|