Research Article
Experimental Study on the Mechanical Properties of the Fiber Cement Mortar Containing Polyurethane
Table 3
Flexural/compression strength ratio of mortar.
| | Number | Flexural/compression strength (MPa) | | 7 days | 14 days | 28 days |
| | P0 | 0.18 | 0.18 | 0.18 | | P5 | 0.29 | 0.27 | 0.22 | | P10 | 0.28 | 0.25 | 0.23 | | P15 | 0.24 | 0.28 | 0.23 | | P20 | 0.23 | 0.28 | 0.20 |
|
|