Research Article
Comparative Study on Cold Compaction Behavior of TiH2 Powder and HDH-Ti Powder
Figure 6
The influence of different compaction pressures on PSD of initial TiH2 powder: (a) 38–63 μm TiH2, (b) 63–88 μm TiH2, and (c) 88–125 μm TiH2. —■—initial powder, —●—powder after compaction (300 MPa), —▲—powder after compaction (450 MPa), and —◆—powder after compaction (600 MPa).
(a) |
(b) |
(c) |