Comparative Study on Cold Compaction Behavior of TiH2 Powder and HDH-Ti Powder
Figure 9
Relative densities (a–d) and parameters (e–h) versus compaction pressure for TiH2 powder and HDH titanium powder. ■—TiH2 38–63 μm, ●—TiH2 88–125 μm, ▲—TiH2 0–63 μm, ▼—TiH2 0–125 μm, □—HDH-Ti 38–63 μm, ○—HDH-Ti 88–125 μm, △—HDH-Ti 0–63 μm, and ▽—HDH-Ti 0–125 μm.