Research Article
[Retracted] Optimizing the Parameters of Zirconium Carbide and Rice Husk Ash Reinforced with AA 2618 Composites
Table 5
Output of the experiments.
| | Standard order units | Run order | A-reinforcement (wt%) | B-speed (m/min) | C-feed (mm/rev) | D-depth of cut (mm) | Ra (μm) | Tool wear (μm) | MRR (g/min) |
| | 19 | 1 | 0 | 210 | 0.6 | 1.5 | 0.98 | 69.6 | 8 | | 23 | 2 | 10 | 190 | 0.4 | 2 | 0.78 | 56 | 14.5 | | 20 | 3 | 20 | 210 | 0.6 | 1.5 | 1.6 | 60.7 | 10 | | 7 | 4 | 10 | 210 | 0.2 | 2 | 1.4 | 31 | 16 | | 17 | 5 | 0 | 210 | 0.2 | 1.5 | 0.92 | 18.6 | 9.5 | | 12 | 6 | 20 | 210 | 0.4 | 2 | 1.41 | 62 | 12.5 | | 8 | 7 | 10 | 210 | 0.6 | 2 | 1.03 | 89.9 | 8 | | 2 | 8 | 20 | 190 | 0.4 | 1.5 | 1.3 | 35 | 9 | | 25 | 9 | 0 | 210 | 0.4 | 1.5 | 1.03 | 41.5 | 11.5 | | 6 | 10 | 10 | 210 | 0.6 | 1 | 1.41 | 29.6 | 15 | | 13 | 11 | 10 | 190 | 0.2 | 1.5 | 0.75 | 17.8 | 15 | | 4 | 12 | 20 | 210 | 0.4 | 1.5 | 0.78 | 42.2 | 7 | | 5 | 13 | 10 | 210 | 0.2 | 1 | 0.55 | 10 | 18.5 | | 24 | 14 | 10 | 230 | 0.4 | 2 | 1.46 | 65 | 8.5 | | 2 | 15 | 10 | 210 | 0.4 | 1.5 | 0.82 | 39.8 | 20 | | 26 | 16 | 10 | 210 | 0.4 | 1.5 | 1.06 | 41.2 | 19 | | 1 | 17 | 0 | 190 | 0.4 | 1.5 | 1.2 | 35.3 | 9.5 | | 15 | 18 | 10 | 190 | 0.6 | 1.5 | 1.22 | 53.9 | 11 | | 14 | 19 | 10 | 230 | 0.2 | 1.5 | 1.25 | 21.8 | 10.5 | | 3 | 20 | 0 | 230 | 0.4 | 1.5 | 1.06 | 42 | 4.5 | | 9 | 21 | 0 | 210 | 0.4 | 1 | 0.85 | 18.8 | 16.5 | | 18 | 22 | 20 | 210 | 0.2 | 1.5 | 0.8 | 20 | 10.5 | | 22 | 23 | 10 | 230 | 0.4 | 1 | 1.02 | 21.56 | 7.5 | | 11 | 24 | 0 | 210 | 0.4 | 2 | 0.65 | 59.58 | 15 | | 10 | 25 | 20 | 210 | 0.4 | 1 | 0.74 | 20 | 11 | | 21 | 26 | 10 | 190 | 0.4 | 1 | 0.65 | 18 | 13 | | 16 | 27 | 10 | 230 | 0.6 | 2 | 1.6 | 65.64 | 4.5 |
|
|