The prior probability distribution of the magnetic-acoustic feature parameters for each fatigue damage state. (a) Cumulative ringing count. (b) Energy (proportion of frequency band 1). (c) Amplitude (singularity index). (d) MSE(Hp(y))avg. (e) MSE(K)avg.