Research Article
Evaluation of Fatigue Behavior of Asphalt Layers Containing Nanosilica Modified Tack Coat
| | Sieve size (mm) | % Passing | Gradation limits (%) |
| | 19 mm | 100 | 100 | | 12.5 mm | 96 | 90–100 | | 9.5 mm | 85 | — | | 4.75 mm (no. 4) | 66.5 | 44–74 | | 2.36 mm (no. 8) | 36.8 | 28–58 | | 0.3 mm (no. 50) | 10 | 7–23 | | 0.075 mm (no. 200) | 4 | 2–10 |
|
|