Research Article
Preparation and Characterization of High Modulus Agent Modified Asphalt and Its High Modulus Mixture
Table 2
Technical indexes of pen # 90 asphalt binder.
| Indicators | Unit | Standard index | Test values | Standard |
| Penetration (25°C, 100 g, 5 s) | 0.1 | 80–100 | 82.9 | T0604 | Softening point | °C | ≥43 | 46.3 | T0606 | Ductility (5 cm/min, 15°C) | cm | ≥100 | 167.3 | T0605 | Dynamic viscosity (60°C) | Pa·s | ≥140 | 162 | T0620 | Relative density (15°C) | g/cm3 | — | 1.034 | T0603 |
| After the thin-film oven test (TFOT) | Loss on heating | %Wt | ≤±0.8 | −0.48 | T0609 | Retained penetration after TFOT | % | ≥57 | 76 | Retained ductility after TFOT | Cm | ≥8 | 10 |
|
|