Heat Index Based Optimisation of Primary Process Parameters in Friction Stir Welding on Light Weight Materials
Table 4
Experimental results on mechanical property (yield strength in MPa).
| Shoulder radius | Tool rotational speed (rpm) | Weld speed | 60 mm/min | 70 mm/min | 80 mm/min |
| 7.5 | 800 | 311.2 | 286.7 | 278.9 | 900 | 303.2 | 300.8 | 287.3 | 1000 | 300.1 | 308.3 | 296.7 | 1100 | 297.3 | 305.6 | 297.1 | 1200 | 294.9 | 301.9 | 308.3 |
| 9 | 800 | 308.8 | 287.4 | 284.7 | 900 | 305.1 | 311.4 | 295.5 | 1000 | 299.5 | 307.2 | 299.2 | 1100 | 299.3 | 303.5 | 312.8 | 1200 | 296.3 | 302.1 | 312.1 |
| 10.5 | 800 | 307.1 | 313.1 | 294.6 | 900 | 300.9 | 311.9 | 313.1 | 1000 | 295.5 | 305.9 | 312.4 | 1100 | 293.3 | 301.3 | 308.1 | 1200 | 292.9 | 300.1 | 304.1 |
| 12 | 800 | 300.1 | 310.1 | 298.5 | 900 | 298.3 | 307.2 | 312.4 | 1000 | 296.5 | 302.9 | 308.3 | 1100 | 294.4 | 301.1 | 304.5 | 1200 | 293.9 | 299.3 | 303.6 |
|
|