Research Article
Experimental Investigation and Parametric Analysis of the Mechanical Properties of Aluminum Alloy Thin-Walled Hollow Columns under Axial Compression
Table 1
Results of tensile tests.
| Number | E/GPa | σ tu/MPa | ε tu/103 | n | ƒ 0.1/MPa | ƒ 0.2/MPa |
| 1-1 | 63.54 | 207.59 | 26.33 | 24.21 | 181.44 | 186.71 | 1-2 | 55.59 | 195.71 | 23.70 | 16.47 | 170.35 | 177.67 | 1–3 | 66.05 | 204.63 | 30.43 | 18.87 | 175.86 | 182.44 | 1–4 | 58.59 | 197.12 | 27.82 | 22.99 | 171.82 | 177.08 | 1–5 | 62.44 | 195.85 | 23.34 | 24.72 | 173.34 | 178.27 | AVE | 61.24 | 200.18 | 26.27 | 21.45 | 174.56 | 180.43 |
|
|