Research Article
Improvement of Mechanical Behavior of FSW Dissimilar Aluminum Alloys by Postweld Heat Treatments
Table 2
Tensile properties of FSW joints at the heat treatment method.
| Heat treatment on samples | Tensile strength, TS (MPa) | Yield strength, YS (MPa) | Elongation (%) |
| HT-0°C | 201.45 | 162.38 | 10.25 | HT-300°C | 199.58 | 152.38 | 15.25 | HT-350°C | 208.26 | 178 | 14.25 | HT-400°C | 200.53 | 158 | 12.34 | HT-450°C | 197.99 | 167 | 12.99 | HT-500°C | 195.36 | 153 | 16.21 |
|
|