Research Article
Study on Decarburization Mechanism and Law of GCr15 Bearing Steel during Heat Treatment
Figure 8
Optical micrographs of decarburized surface of Cr15 bearing steel heated at the temperature of 800°C for (a) 20 min, (b) 30 min, (c) 40 min, (d) 50 min, (e) 60 min, and (f) 70 min. Scale bar corresponds to 100 μm.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |