| Lithology | Density ρ (g/cm3) | Modulus of elasticity E (GPa) | Poisson’s ratio | Tensile strength σt (MPa) | Cohesive force C (MPa) | Angle of internal friction Φ (°) |
| Bluish grey dolomite | 2.85 | 20.0149 | 0.269 | 2.1966 | 2.6110 | 41.99 | Faded dolomite | 2.84 | 13.0620 | 0.280 | 2.1796 | 2.5504 | 34.05 | Orebody | 2.84 | 17.8847 | 0.214 | 2.2577 | 2.9637 | 47.42 | Purple slate | 2.63 | 4.5676 | 0.284 | 1.0431 | 1.5710 | 31.68 | Carbonaceous slate | 2.70 | 2.2416 | 0.350 | 0.9298 | 1.3848 | 35.42 |
|
|