Research Article
Wear Investigation of Aluminum Alloy Surface Layers Fabricated through Friction Stir Welding Method
| Considerations | Dof | SS | MS | F | P value | Contribution level (%) |
| LD | 2 | 0.000134 | 0.000067 | 72.02 | 0.000 | 83.75 | SE | 2 | 0.000006 | 0.000003 | 3.40 | 0.085 | 3.75 | SS | 2 | 0.000003 | 0.000002 | 1.68 | 0.246 | 1.85 | LDSE | 4 | 0.000004 | 0.000001 | 1.08 | 0.428 | 2.12 | LDSS | 4 | 0.000002 | 0.000001 | 0.55 | 0.704 | 1.25 | SESS | 4 | 0.000003 | 0.000001 | 0.79 | 0.563 | 1.85 | Residual error | 8 | 0.000007 | 0.000001 | | | 5.43 | Total | 26 | 0.000160 | | | | |
|
|