Research Article
Experimental Investigation of Heat-Treated Tool on Wire Electric Discharge Machining of Titanium Alloy (Ti-6Al-4V)
Table 13
Determination of performance matrix.
| Exp. | MRR | TWR | Ra | Recast layer thickness |
| L1 | 0.222 | 3.0555 | 3.9952 | 0.3327 | L2 | 0.1946 | 2.8224 | 4.4327 | 0.1802 | L3 | 0.1509 | 1.8868 | 6.0951 | 0.1963 | L4 | 0.4441 | 3.849 | 4.6747 | 0.3235 | L5 | 0.3303 | 3.0238 | 4.6796 | 0.3627 | L6 | 0.5915 | 1.0353 | 4.9992 | 0.288 | L7 | 0.5333 | 4.9777 | 4.7921 | 0.4032 | L8 | 0.1439 | 1.3087 | 4.1095 | 0.2954 | L9 | 0.1363 | 1.4366 | 6.6128 | 0.3452 | SOS | 1.08981291 | 74.44606232 | 225.0855097 | 0.869837 |
|
|