Research Article
Experimental Investigation of Heat-Treated Tool on Wire Electric Discharge Machining of Titanium Alloy (Ti-6Al-4V)
Table 14
Normalized decision matrix.
| Exp. | MRR | TWR | Ra | Recast layer thickness |
| L1 | 0.212655686 | 0.354128942 | 0.266296069 | 0.356725259 | L2 | 0.186408994 | 0.327112920 | 0.295457195 | 0.193212779 | L3 | 0.144548392 | 0.218677954 | 0.406262809 | 0.210475408 | L4 | 0.425407164 | 0.446094681 | 0.311587464 | 0.346860900 | L5 | 0.316397177 | 0.350454949 | 0.311914069 | 0.388891649 | L6 | 0.566602876 | 0.119990081 | 0.333216688 | 0.308797339 | L7 | 0.510852602 | 0.576909716 | 0.319412644 | 0.432316275 | L8 | 0.137843033 | 0.151676828 | 0.273914622 | 0.316731715 | L9 | 0.130562928 | 0.166500291 | 0.440769586 | 0.370127922 |
|
|