Experimental Investigation of Heat-Treated Tool on Wire Electric Discharge Machining of Titanium Alloy (Ti-6Al-4V)
Table 16
Weighted normalized matrix.
| Exp. | MRR | TWR | Ra | Recast layer thickness |
| L1 | 0.053163922 | 0.088532236 | 0.066574017 | 0.089181315 | L2 | 0.046602248 | 0.08177823 | 0.073864299 | 0.048303195 | L3 | 0.036137098 | 0.054669488 | 0.101565702 | 0.052618852 | L4 | 0.106351791 | 0.11152367 | 0.077896866 | 0.086715225 | L5 | 0.079099294 | 0.087613737 | 0.077978517 | 0.097222912 | L6 | 0.141650719 | 0.02999752 | 0.083304172 | 0.077199335 | L7 | 0.127713150 | 0.144227429 | 0.079853161 | 0.108079069 | L8 | 0.034460758 | 0.037919207 | 0.068478655 | 0.079182929 | L9 | 0.032640732 | 0.041625073 | 0.110192396 | 0.092531980 |
|
|