Research Article
Experimental Investigation of Heat-Treated Tool on Wire Electric Discharge Machining of Titanium Alloy (Ti-6Al-4V)
Table 4
Determination of performance matrix.
| Exp. | MRR | TWR | Ra | Recast layer thickness |
| L1 | 0.0554 | 4.125 | 5.0444 | 0.2214 | L2 | 0.2297 | 3.0982 | 6.378 | 0.2923 | L3 | 0.1575 | 2.1325 | 5.301 | 0.3277 | L4 | 0.2307 | 3.9872 | 5.135 | 0.1742 | L5 | 0.1758 | 3.5280 | 5.4437 | 0.2982 | L6 | 0.1060 | 2.9682 | 4.0937 | 0.4669 | L7 | 0.2666 | 5.6324 | 6.8372 | 0.2337 | L8 | 0.1083 | 2.5554 | 4.6398 | 0.5074 | L9 | 0.1097 | 1.9895 | 5.2216 | 0.5280 | SOS | 0.27084017 | 110.5288927 | 262.5260852 | 1.16996348 |
|
|