Research Article
Experimental Investigation of Heat-Treated Tool on Wire Electric Discharge Machining of Titanium Alloy (Ti-6Al-4V)
Table 5
Normalized decision matrix.
| Exp. | MRR | TWR | Ra | Recast layer thickness |
| L1 | 0.106451853 | 0.39236119 | 0.311331659 | 0.204687567 | L2 | 0.441371672 | 0.294694167 | 0.393639149 | 0.270235663 | L3 | 0.302638391 | 0.202838846 | 0.327168568 | 0.302963486 | L4 | 0.443293186 | 0.379253948 | 0.316923335 | 0.16105047 | L5 | 0.33780209 | 0.335575825 | 0.335975766 | 0.2756903 | L6 | 0.203680441 | 0.282328845 | 0.252656096 | 0.43165594 | L7 | 0.512275524 | 0.535741859 | 0.42198018 | 0.216059098 | L8 | 0.208099922 | 0.24306419 | 0.286360445 | 0.469098787 | L9 | 0.210790041 | 0.189236991 | 0.322268137 | 0.488143791 |
|
|