Experimental Investigation of Heat-Treated Tool on Wire Electric Discharge Machining of Titanium Alloy (Ti-6Al-4V)
Table 7
Weighted normalized matrix.
| Exp. | MRR | TWR | Ra | Recast layer thickness |
| L1 | 0.026612963 | 0.098090298 | 0.077832915 | 0.051171892 | L2 | 0.110342918 | 0.073673542 | 0.098409787 | 0.067558916 | L3 | 0.075659598 | 0.050709711 | 0.081792142 | 0.075740871 | L4 | 0.110823296 | 0.094813487 | 0.079230834 | 0.040262618 | L5 | 0.084450522 | 0.083893956 | 0.083993941 | 0.068922575 | L6 | 0.05092011 | 0.070582211 | 0.063164024 | 0.107913985 | L7 | 0.128068881 | 0.133935465 | 0.105495045 | 0.054014775 | L8 | 0.052024981 | 0.060766048 | 0.071590111 | 0.117274697 | L9 | 0.05269751 | 0.047309248 | 0.080567034 | 0.122035948 |
|
|