Research Article
Characterization of PVA Fiber-Reinforced Pervious Concrete with Blended Recycled Ceramic Aggregates and Natural Aggregate
Table 2
Mix proportions of RCCAPC and PVA fiber-reinforced RCCAPC.
| sample | Volume replacement rate/(%) | Cement/(kg·m−3) | RCCA/(kg·m−3) | NCA/(kg·m−3) | Water/(kg·m−3) | PVA fiber content/(%) | Mixing amount/(kg·m−3) |
| RCCA0 | 0 | 351 | 0 | 1481 | 105 | 0 | 0 | RCCA20 | 20 | 358 | 260 | 1185 | 107 | 0 | 0 | RCCA40 | 40 | 365 | 520 | 889 | 109 | 0 | 0 | RCCA60 | 60 | 373 | 780 | 592 | 112 | 0 | 0 | RCCA80 | 80 | 380 | 1040 | 296 | 114 | 0 | 0 | RCCA100 | 100 | 388 | 1300 | 0 | 117 | 0 | 0 | RCCA40F0.1 | 40 | 373 | 780 | 592 | 112 | 0.1 | 1.12 | RCCA40F0.15 | 40 | 373 | 780 | 592 | 112 | 0.15 | 1.68 | RCCA40F0.2 | 40 | 373 | 780 | 592 | 112 | 0.2 | 2.24 | RCCA40F0.25 | 40 | 373 | 780 | 592 | 112 | 0.25 | 2.8 | RCCA40F0.3 | 40 | 373 | 780 | 592 | 112 | 0.3 | 3.36 | RCCA40F0.35 | 40 | 373 | 780 | 592 | 112 | 0.35 | 3.92 |
|
|
RCCA20-volume replacement ratio of RCCA is 20%; RCCA40F0.1-volume replacement ratio of RCCA is 40%, and the PVA fiber volume content is 0.1%.
|