Examination of Friction Stir-Welded AA 6262/5456 Joints through the Optimization Technique
Table 5
Welding efficiency-tensile strength.
| Al5456/Al6262 FSW samples | Tensile strength (MPa) | Weld joint efficiency with Al5456 (A/B) x 100 in (%) | Weld joint efficiency with Al5456 (in (%)) (A/C) x 100 in (%) | Al5456/Al6262 composites (A) | Al5456 alloy (B) | Al6262 alloy (C) |
| L1 | 192.65 | 305 | 260 | 63.16393 | 74.09615 | L2 | 193.28 | 305 | 260 | 63.37049 | 74.33846 | L3 | 189.54 | 305 | 260 | 62.14426 | 72.9 | L4 | 179.38 | 305 | 260 | 58.81311 | 68.99231 | L5 | 197.84 | 305 | 260 | 64.86557 | 76.09231 | L6 | 187.92 | 305 | 260 | 61.61311 | 72.27692 | L7 | 195.68 | 305 | 260 | 64.15738 | 75.26154 | L8 | 194.77 | 305 | 260 | 63.85902 | 74.91154 | L9 | 196.27 | 305 | 260 | 64.35082 | 75.48846 | L10 | 175.53 | 305 | 260 | 57.55082 | 67.51154 | L11 | 186.64 | 305 | 260 | 61.19344 | 71.78462 | L12 | 169.29 | 305 | 260 | 55.50492 | 65.11154 | L13 | 170.58 | 305 | 260 | 55.92787 | 65.60769 | L14 | 171.29 | 305 | 260 | 56.16066 | 65.88077 | L15 | 165.88 | 305 | 260 | 54.38689 | 63.8 | L16 | 196.89 | 305 | 260 | 64.5541 | 75.72692 | L17 | 195.76 | 305 | 260 | 64.18361 | 75.29231 | L18 | 189.79 | 305 | 260 | 62.22623 | 72.99615 | L19 | 174.88 | 305 | 260 | 57.3377 | 67.26154 | L20 | 199.26 | 305 | 260 | 65.33115 | 76.63846 | L21 | 186.84 | 305 | 260 | 61.25902 | 71.86154 | L22 | 202.44 | 305 | 260 | 66.37377 | 77.86154 | L23 | 183.52 | 305 | 260 | 60.17049 | 70.58462 | L24 | 179.29 | 305 | 260 | 58.78361 | 68.95769 | L25 | 181.99 | 305 | 260 | 59.66885 | 69.99615 | L26 | 195.37 | 305 | 260 | 64.05574 | 75.14231 | L27 | 193.78 | 305 | 260 | 63.53443 | 74.53077 |
|
|