Research Article
Recycled Coarse Aggregate for Sustainable Self-Compacting Concrete and Mortar
| Mix designation | Falling ability | Passing ability | Segregation resistance | Slump flow (SF) (mm) | Slump flow time T50 (sec) | V-funnel flow time Tv (sec) | J-ring flow (JF) mm | Blocking index BI (mm) | J-ring BJ (mm) | L-box H2/H1 | Segregation index, SI (%) |
| NCASCC | 720 | 2 | 9.6 | 700 | 20 | 6.0 | 0.84 | 9.73 | RCASCC-25 | 695 | 3.42 | 10.27 | 673 | 22 | 7.0 | 0.82 | 9.51 | RCASCC-50 | 685 | 4.14 | 10.91 | 670 | 15 | 8.0 | 0.81 | 9.01 | RCASCC-100 | 680 | 4.72 | 11.47 | 665 | 15 | 9.5 | 0.80 | 8.08 |
|
|