Research Article
Durability Capacity Change of Rubber Powder Composite BRA Modified Asphalt Mixture
Table 7
Results of rutting test of mixture.
| Specimen number | 1# | 2# | 3# | 4# | 5# | 6# | 1 | 2 | 1 | 2 | 1 | 2 | 1 | 2 | 1 | 2 | 1 | 2 |
| d1 (mm) | 3.800 | 2.165 | 1.374 | 1.836 | 2.133 | 2.084 | 2.668 | 1.704 | 1.704 | 2.300 | 1.145 | 1.732 | d2 (mm) | 4.214 | 2.412 | 1.480 | 1.971 | 2.280 | 2.285 | 2.854 | 1.895 | 1.802 | 2.479 | 1.241 | 1.832 | DS (times/mm) | 1522 | 2551 | 5943 | 4667 | 4286 | 3134 | 3387 | 3298 | 6429 | 3520 | 6562 | 6300 | DS (times/mm) | 2036 | 5305 | 3710 | 3343 | 3520 | 6431 |
|
|