Research Article

Adhesion Enhancement on a Duplex DLC HiPIMS Positive Pulse Coating Performed by Active Screen Plasma Nitriding Pretreatment on 316L Stainless Steel Substrate

Figure 7

Experimental data derived from the scratch test with the corresponding values of critical load (LC2 and LC3) for DLC WC : C coating sample.