Research Article

Adhesion Enhancement on a Duplex DLC HiPIMS Positive Pulse Coating Performed by Active Screen Plasma Nitriding Pretreatment on 316L Stainless Steel Substrate

Table 2

Summary of the experimental data of volume loss and wear coefficient measured by confocal microscopy.

Types of samplesWidth of wear track (μm)Wear coefficient (mm3 Nm−1)

DLC WC : C110 ± 54.0 ± 1.0 × 10−7
ASPN 350°C + DLC WC : C80 ± 2.54.5 ± 2.4 × 10−7
ASPN 400°C + DLC WC : C80 ± 2.57.9 ± 3.7 × 10−7