Research Article

[Retracted] Experimental Investigation on the Average Surface Roughness (Ra) of AlSi10Mg Alloy Manufactured by Laser Powder Bed Fusion Method

Table 2

Process parameters used for aluminium samples.

ParameterCondition

Power (P) (W)175–375
Scan speed (mm/sec)400–1000
Hatch distance (mm)0.10–0.14
Energy density (J/mm3)54.2–114.6