Research Article
[Retracted] Composite Nano-Calcium-Based Material for Reinforcement and Protection of Earthen Ruins in Humid Environment
Table 2
Compressive strength at different ages.
| Density (g·cm3) | a-solid content (%) | Compressive strength (MPa) | 3 d | 7 d | 14 d | 28 d | 90 d |
| 1.55 | 0 | 0.26 | 0.37 | 0.46 | 0.57 | 0.64 | 0.2 | 0.33 | 0.46 | 0.62 | 0.69 | 0.71 | 0.4 | 0.43 | 0.52 | 0.69 | 0.70 | 0.80 |
| 1.65 | 0 | 0.53 | 0.53 | 0.67 | 0.70 | 0.72 | 0.2 | 0.79 | 0.79 | 1.09 | 1.11 | 1.16 | 0.4 | 0.92 | 0.98 | 1.13 | 1.26 | 1.30 |
| 1.75 | 0 | 0.93 | 0.93 | 1.35 | 1.84 | 1.88 | 0.2 | 1.03 | 1.13 | 1.71 | 1.88 | 2.00 | 0.4 | 1.27 | 1.27 | 2.05 | 2.20 | 2.22 |
|
|