[Retracted] Composite Nano-Calcium-Based Material for Reinforcement and Protection of Earthen Ruins in Humid Environment
Table 5
Compressive strength after salt resistance test.
| Density (g cm3) | Compressive strength (MPa) | a-0% | a-0.2% | a-0.4% |
| 1.55 | The first loop break | Breaking the fifth cycle | 0.70 | 1.65 | The third loop break | 0.30 | 0.86 | 1.75 | The third loop break | 0.46 | 1.50 |
|
|