Research Article
Microstructure and Properties of Super-Ferritic Stainless Steels Used for Marine Construction after Fire Exposure
Figure 6
The surface morphologies of representative samples after immersion corrosion: (a), (b) immersion for 24 h of samples soaking for 4h at 600°C, (c, d) immersion for 24 h of samples soaking for 4h at 800°C.
(a) |
(b) |
(c) |
(d) |